Welding characteristics of titanium and its alloys

1 Physical and chemical properties of titanium and its alloys Titanium has two allotropes, represented by and , respectively, with a transition temperature of 882.5 degree , its low-temperature crystal is a close-packed hexagonal lattice, and stable above 882.5 degree The crystal is a body-centered cubic lattice. Titanium has poor thermal conductivity and its thermal conductivity is slightly lower than that of stainless steel. When there are impurities in titanium, its thermal conductivity decreases. Table 1 lists the comparison of the main physical properties of industrial pure titanium and other metal materials.

2 Welding structure of titanium alloy

The welded structure of industrial pure titanium and the titanium alloy is single-phase at room temperature, and a zigzag or needle-like structure is formed depending on the cooling rate. Various mechanical properties have no major changes compared with the base metal, and the welding performance is good. In the process of cooling from phase, plus titanium alloy forms martensite ( ' phase), and the quantity and properties of ' phase change according to alloy composition and cooling rate. In general, with the increase of the phase, the ductility and toughness of the alloy decrease. Even for Ti-6Al-4V with good weldability, when the content of -stabilizing element vanadium is more than 5 percent , the weldability decreases. The martensite formation temperature of beta titanium alloy is lower than room temperature, and the weld is in a metastable beta phase, so the weldability does not deteriorate. However, due to the addition of too many alloying elements, extensibility is often lacking. In addition, aging and cold working increase the strength of the alloy, while welding will cause a loss of strength, so welding is not used for titanium alloy processing.


titanium supplier

3 Welding defects of titanium alloys

3.1 Embrittlement in the welded joint area

The welding area of titanium and titanium alloys is susceptible to contamination by impurities such as gas and embrittlement. The main elements causing embrittlement are O, N, H, C, etc. Titanium and titanium alloys are relatively stable at room temperature, but as the temperature increases, the ability of titanium and titanium alloys to absorb O, N, and H also increases significantly. Ti starts to absorb hydrogen from 250 degree , oxygen from 400 degree , and nitrogen from 600 degree . Nitrogen and oxygen have a great influence on joint strength and bending plasticity. With the increase of nitrogen and oxygen content in the weld, the joint strength increases and the bending plasticity decreases, and the effect of nitrogen is greater than that of oxygen. Hydrogen mainly affects the impact toughness of the joint.

3.2 Welding zone crack tendency

(1) Hot cracks.

Since titanium and titanium alloys contain fewer impurities such as S, P, and C, few low-melting-point eutectics are formed at the grain boundaries, and the crystallization temperature range is very narrow, and the shrinkage of the weld is small when it solidifies, so the sensitivity to hot cracks is high. Low.

(2) Cold cracks and delayed cracks.

When the content of oxygen and nitrogen in the weld is high, the weld performance becomes brittle, and cracks will appear under the action of greater welding stress, which is formed at lower temperatures.

When welding titanium alloys, delayed cracks sometimes appear in the heat-affected zone, and hydrogen is the main reason for the formation of delayed cracks. The main method to prevent delayed cracking is to reduce the source of hydrogen at the welded joints, and if necessary, vacuum annealing can be performed to reduce the hydrogen content of the welded joints.

3.3 Weld pores

Porosity is a common defect in the welding of titanium and titanium alloys. O2, N2, H2, CO2, and H2O may all cause porosity. The pores of titanium and titanium alloy welds are mostly distributed near the fusion zone, which is a feature of the pores of titanium and titanium alloys. The pores in the weld not only cause stress concentration, but also reduce the plasticity of the metal around the pores, and even lead to the fracture of the entire welded joint. Therefore, the formation of pores must be strictly controlled.